. Scanning tunneling microscopy image of hydrogenated graphene (A:ortho-dimers, B:para-dimers, C ... and 50 hours reversing the conversion. -1 ★ red shift in D peak, from 1350 cm -1 to 1330 cm -1 ... gradient observed with electrochemical conversion of graphene on semi-insulating Si-face SiC ★ red