산화물 피복강재의 밀착성과 내식성에 관한 연구 ( 2 )
(주)코리아스칼라
- 최초 등록일
- 2023.04.05
- 최종 저작일
- 1996.08
- 8페이지/ 어도비 PDF
- 가격 4,000원
* 본 문서는 배포용으로 복사 및 편집이 불가합니다.
서지정보
ㆍ발행기관 : 한국수산해양기술학회(구 한국어업기술학회)
ㆍ수록지정보 : 수산해양기술연구 / 32권 / 3호
ㆍ저자명 : 임우조, 이종락
영어 초록
To improve the corrosion resistance of stainless steel and Fe, the adherence between fIlm and substarte and the corrosion resistance to ceramic fIlm (TiO2 and ZrO2), coated by RF magnetron sputtering, were studied. The adherence index (X) was determined by the measure of micro - hardness test. Also, the corrosion resistance on oxide coatings was studied using electrochemical measurement. The main results obtained are as the following: 1) In the micro - hardness test, with 1J.UI1 thickness fIlm, it has only one the value of X. Above 2J.UI1 thickness fIlm, however, get another value ofX as the cracks in fIlm. 2) The adhensivity of titania (TiO2) coated fIlm is superior to that of zirconia (ZrO2) coated fIlm. 3) All oxide fIlm used adhere well on the mild materials such as pure steel than high intensity materials like stainless steel. 4) The corrosion resistance of zirconia coated materials was improved compared to titania coated materials.
참고 자료
없음
"수산해양기술연구"의 다른 논문
더보기 (5/10)