Activated Carbon Fibers from Chemically Modified Coal Tar Pitchs
(주)학지사
- 최초 등록일
- 2015.03.24
- 최종 저작일
- 2000.01
- 6페이지/ 어도비 PDF
- 가격 3,000원
* 본 문서는 배포용으로 복사 및 편집이 불가합니다.
서지정보
ㆍ발행기관 : 한국탄소학회
ㆍ수록지정보 : Carbon Letters / 1권 / 1호
ㆍ저자명 : S.K.RYN, J.W. Shim, K.S.Yang and I.Mochida
목차
1.Introduction
2.Experiment
3.Results and Disussion
4. Conclusion
References
한국어 초록
Coal tar pitch was chmically modified 10wt% benzoquinone(BQ) to raise the softening point of isotropic pitch pre-cursor and the precursor was melt-spun into fibers, stabilizd, carbonized and activated with steam at 900'C. The weight loss of carbon fiber-benzoquinone (CF-BQ) increased with the increase of activation time like other fibers, but was lower than those of Kureha fiber at the same activation time in spite of larger geometric surface area.
영어 초록
Coal tar pitch was chmically modified 10wt% benzoquinone(BQ) to raise the softening point of isotropic pitch pre-cursor and the precursor was melt-spun into fibers, stabilizd, carbonized and activated with steam at 900'C. The weight loss of carbon fiber-benzoquinone (CF-BQ) increased with the increase of activation time like other fibers, but was lower than those of Kureha fiber at the same activation time in spite of larger geometric surface area.