Microstructure, electric, and thermal properties of the Ta-Cu composite is evaluated for the application in electric contact materials. This material..
metallic glass is fabricated using gas-atomized Al82Ni7Co3Y8 metallic glass powder and subsequent spark plasma ... From these results, we conclude that the Z-position-controlled spark plasma sintering process, using
Two sintering methods of a pressureless sintering and a spark-plasma sintering are tested to densify ... Spark-plasma sintering is carried out under the following condition: sintering temperature of 1050oC, ... Spark-plasma sintering at 1050oC for 10 min exhibits nearly complete densification of 98.6% relative
Bismuth antimony telluride (BiSbTe) thermoelectric materials were successfully prepared by a spark plasma ... Spark plasma sintering was applied on the BiSbTe powders at 240, 320, and 380˚C, respectively, under